Effect of electrical discharge machining on dental Y-TZP ceramic-resin bonding

Basit öğe kaydını göster

dc.contributor.author Rona, Nergiz
dc.contributor.author Yenisey, Murat
dc.contributor.author Küçüktürk, Gökhan
dc.contributor.author Gürün, Hakan
dc.contributor.author Çoğun, Can
dc.contributor.author Esen, Ziya
dc.date.accessioned 2020-03-18T08:02:13Z
dc.date.available 2020-03-18T08:02:13Z
dc.date.issued 2017-04
dc.identifier.citation Rona, Nergiz...et.al. (2017). "Effect of electrical discharge machining on dental Y-TZP ceramic-resin bonding", Journal Of Prosthodontic Research, Vol.61, No.2, pp.158-167. tr_TR
dc.identifier.issn 1883-1958
dc.identifier.uri http://hdl.handle.net/20.500.12416/2664
dc.description.abstract Purpose: The study determined (i) the effects of electrical discharge machining (EDM) on the shear-bond strength (SBS) of the bond between luting resin and zirconia ceramic and (ii) zirconia ceramic's flexural strength with the three-point bending (TPB) test. Methods: Sixty 4.8 mm x 4.8 mm x 3.2 mm zirconia specimens were fabricated and divided into four groups (n = 15): SBG: sandblasted + silane, TSCG: tribochemical silica coated + silane, LTG: Er:YAG laser treated + silane, EDMG: EDM + silane. The specimens were then bonded to a composite block with a dual-cure resin cement and thermal cycled (6000 times) prior to SBS testing. The SBS tests were performed in a universal testing machine. The SBS values were statistically analyzed using ANOVA and Tukey's test. To determine flexural strength, sixty zirconia specimens were prepared and assigned to the same groups (n = 15) mentioned earlier. After surface treatment TPB tests were performed in a universal testing machine (ISO 6872). The flexural strength values were statistically analyzed using ANOVA and Tukey's test (a = 0.05). Results: The bond strengths for the four test groups (mean SD; MPa) were as follows: SBG (Control), 12.73 +/- 3.41, TSCG, 14.99 +/- 3.14, LTG, 7.93 +/- 2.07, EDMG, 17.05 +/- 2.71. The bond strength of the EDMG was significantly higher than those of the SBG and LTG (p < 0.01). The average flexural strength values for the groups SBG (Control), TSCG, LTG and EDMG were 809.47, 800.47, 679.19 and 695.71 MPa, respectively (p > 0.05). Conclusions: The EDM process improved the SBS. In addition, there was no significant adverse effect of EDM on the flexural strength of zirconia. tr_TR
dc.language.iso eng tr_TR
dc.publisher Elsevier Ireland LTD tr_TR
dc.relation.isversionof 10.1016/j.jpor.2016.07.006 tr_TR
dc.rights info:eu-repo/semantics/closedAccess tr_TR
dc.subject Zirconia Ceramic tr_TR
dc.subject Electrical Discharge Machining tr_TR
dc.subject Bonding Strength tr_TR
dc.subject Flexural Strength tr_TR
dc.subject Graphite Powder tr_TR
dc.title Effect of electrical discharge machining on dental Y-TZP ceramic-resin bonding tr_TR
dc.type article tr_TR
dc.relation.journal Journal Of Prosthodontic Research tr_TR
dc.contributor.authorID 3837 tr_TR
dc.contributor.authorID 52373 tr_TR
dc.identifier.volume 61 tr_TR
dc.identifier.issue 2 tr_TR
dc.identifier.startpage 158 tr_TR
dc.identifier.endpage 167 tr_TR
dc.contributor.department Çankaya Üniversitesi, Mühendislik Fakültesi, Mekatronik Mühendisliği; Mazleme Bilimi ve Mühendisliği Bölümü tr_TR


Bu öğenin dosyaları:

Dosyalar Boyut Biçim Göster

Bu öğe ile ilişkili dosya yok.

Bu öğe aşağıdaki koleksiyon(lar)da görünmektedir.

Basit öğe kaydını göster